Thermal Insulation Bricks are made of high-quality and high-purity refractory powder, according to the specific gravity of the product, adding organic composite filler, and preparing lightweight mullite products by vacuum extrusion molding and high-temperature sintering finishing.Insulation Bricks gains typical advantages including low thermal conductivity, fine thermal shock resistance, low heat containment and low iron content,Meanwhile,the outstanding mechanical flexibility, coupled with high insulating efficiency expands the extensive applications of IFB in a variety of industrial markets.
Features
- Low thermal conductivity
- High purity and low iron content
- Good thermal resistance with direct access to fire
- Superior thermal shock resistance
- Accurate dimension and easy cutting
Typical Applications
Cracking furnace
01
Conversion furnace
02
Heating equipment
03
Refining equipment
04
Reproduction equipment
Hot blast stove
05
Technical Data
|
Description |
Grade 23 |
Grade 26 |
Grade 28 |
Grade 30 |
|
|
Classification Temperature |
1300C/2300F |
1400C/2600F |
1500C/2732F |
1550C/2822F |
|
|
Density(kg/m3) |
600 |
800 |
900 |
1000 |
|
|
Cold Crushing Strength (MPa) |
1.2 |
1.8 |
2.5 |
3.3 |
|
|
Modulus of Rupture(MPa) |
1.0 |
1.7 |
2.3 |
3.1 |
|
|
Permanent Linear Change (%)x24hrs |
≤0.6 |
≤0.6 |
≤0.8 |
≤0.9 |
|
|
Thermal Expansion (%)1000C |
0.5 |
0.52 |
0.52 |
0.53 |
|
|
Thermal Conductivity (W/m.k) |
350C |
0.18 |
0.25 |
0.33 |
0.38 |
|
400C |
0.20 |
0.29 |
0.35 |
0.40 |
|
|
600C |
0.24 |
0.32 |
0.37 |
0.42 |
|
|
Chemical Composition (%) |
Al2O3 |
42 |
56 |
67 |
73 |
|
SiO2 |
55 |
41 |
30 |
24 |
|
|
Fe2O3 |
≤1 |
≤0.8 |
≤0.7 |
≤0.7 |
|
|
K2O+Na2O |
1.1 |
1.7 |
1.7 |
1.7 |
|
Packing and shipping

FAQ